Surface hardening

Carburising   3 of 5
 

Carburising involves the diffusion of carbon into the surface layers of a low carbon steel at high temperatures. Controlled cooling after carburising (water, oil or polymer quenching) produces hard martensitic layers at the surface (this is due to the increased hardenability of the carbon enriched surface region).

 

 

 