Question Which of the following products is produced by deep drawing?

 

Green tick Stainless steel sink- Correct.

Red cross Car bonnet- Incorrect , this is stretch formed.  Try again.

Red cross Car wheel arch - Incorrect , this is  produced by a combination of drawing and stretch forming.  Try again.

Green tick Beverage drinks can - Correct

Green tick Fire fighters helmets -Correct  (these are deep drawn and covered with leather).

Red cross Try again.

    

Click on your answer to check.

 