The surface hardness of a component such as a gear is important in determining the life of the component since the surface hardness is related to the wear resistance of the material. The surface hardness can be controlled by a number of processes:
Controlled alloying additions to the steel Controlled heat treatmentCarburisingNitriding Carbo-nitriding