Calculating the angle between two planes
For cubic crystals, the angle, f between two planes, (h1 k1 l1)
and (h2 k2 l2)
is given by:

Example:
| Calculate the angle between the (111) and (200) planes. From the above,


which produces the result, f = 54.75°. |

|