We shall conduct an experiment to determine how the extension of a spring varies with the stretching force.

A spring is hung vertically from a fixed point and a force is applied in stages by hanging weights from the spring.

The apparatus is set up as shown. For the purposes of this experiment we shall be using loads of 100g, and the extension of the spring shall be measured in metres.

definitions.gif (2989 bytes)
Each kilogram of mass on Earth has a weight of approximately 9.8 Newtons.

Hookes_law_apparatus_labelled.jpg (11061 bytes)

questions.gif (805 bytes)
Approximately how much force does a 100g load exert on the spring?

9.8N
100N
0.98N
9800N

 